Investigating Effect of Bearing Length on Tensile Strength of 1045 Steel in Wire Drawing Operation

Abstract

In this work, effect of bearing length on tensile strength was investigated. The influence of the bearing length is illustrated using two different reduction ratios and wire diameters. According to the results, the increase in strength was observed as the length of the bearing zone increased. However, the long bearing length caused various manufacturing problems during production. Microhardness distributions in wire cross section, on the other hand, increased as the length of bearing increased. The main reason for the increase of microhardness is the deformation hardening caused by the high friction force obtained by increasing the bearing length.

Keywords

Kaynakça

  1. Gillström, P., & Jarl, M. (2007). Wear of die after drawing of pickled or reverse bent wire rod. Wear, 262(7–8), 858–867. https://doi.org/10.1016/j.wear.2006.08.016
  2. Korchunov, A., Gun, G., & Polyakova, M. (2014). Recovery effect in drawing of steel bar for sizing. Procedia Engineering, 81, 676–681. https://doi.org/10.1016/j.proeng.2014.10.059
  3. Nilsson, M., & Olsson, M. (2011). Tribological testing of some potential PVD and CVD coatings for steel wire drawing dies. Wear, 273(1), 55–59. https://doi.org/10.1016/j.wear.2011.06.020
  4. Sas-Boca, I. M., Tintelecan, M., Pop, M., Iluţiu-Varvara, D. A., & Mihu, A. M. (2017). The Wire Drawing Process Simulation and the Optimization of Geometry Dies. Procedia Engineering, 181, 187–192. https://doi.org/10.1016/j.proeng.2017.02.368
  5. Schade, P. (2006). Wire drawing failures and tungsten fracture phenomena. International Journal of Refractory Metals and Hard Materials, 24(4), 332–337. https://doi.org/10.1016/j.ijrmhm.2005.09.003
  6. Wei, D., Min, X., Hu, X., Xie, Z., & Fang, F. (2020). Microstructure and mechanical properties of cold drawn pearlitic steel wires: Effects of drawing-induced heating. Materials Science and Engineering A, 784, 139341. https://doi.org/10.1016/j.msea.2020.139341
  7. Xu, P., Liang, Y., Li, J., & Meng, C. (2019). Further improvement in ductility induced by the refined hierarchical structures of pearlite. Materials Science and Engineering A, 745, 176–184. https://doi.org/10.1016/j.msea.2018.12.069

Ayrıntılar

Birincil Dil

İngilizce

Konular

Makine Mühendisliği

Bölüm

Araştırma Makalesi

Yayımlanma Tarihi

3 Aralık 2020

Gönderilme Tarihi

25 Ağustos 2020

Kabul Tarihi

10 Eylül 2020

Yayımlandığı Sayı

Yıl 2020 Cilt: 23 Sayı: 4

Kaynak Göster

APA
Çelik, E., Özen, F., İlhan, E., & Aslanlar, S. (2020). Investigating Effect of Bearing Length on Tensile Strength of 1045 Steel in Wire Drawing Operation. Kahramanmaraş Sütçü İmam Üniversitesi Mühendislik Bilimleri Dergisi, 23(4), 227-235. https://doi.org/10.17780/ksujes.784544

DİZİNLENME ve ARŞİVLEME

download?token=eyJhdXRoX3JvbGVzIjpbXSwiZW5kcG9pbnQiOiJqb3VybmFsIiwib3JpZ2luYWxuYW1lIjoiaW1hZ2UucG5nIiwicGF0aCI6IjAzNTkvYmZjYS81YjQyLzY5ZjFkM2E4NWY2YWY3Ljg1NjQ2NDgxLnBuZyIsImV4cCI6MTc3NzQ1OTY0MCwibm9uY2UiOiI1NTUzYmJiN2U5NGNkMjdkYWNhMTRlMDZiYjc1OTY4NCJ9.nCVoSJClEIC9bWK5gGCmjHyTNRz2N0DhYKVJzJZR9Bs

 

download?token=eyJhdXRoX3JvbGVzIjpbXSwiZW5kcG9pbnQiOiJqb3VybmFsIiwib3JpZ2luYWxuYW1lIjoiaW1hZ2UucG5nIiwicGF0aCI6Ijg5YmUvODZlOC8wYzY0LzY5ZjFkNWE4MWJmYzY0LjM0OTM2NzM1LnBuZyIsImV4cCI6MTc3NzQ2MDE1Miwibm9uY2UiOiI3OWE1Mzk0OWRhMTk0Mjg0OGYzZTUxOWQyNTU5MjdjMSJ9.XxqhJ36woCZcO1DV_I9Mogpgg86-bwM454jQiOcqpS0 

Bu eser, Creative Commons Atıf 4.0 Uluslararası Lisansı ile lisanslanmıştır.